Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 6.94 J/cm @Thickness 12.7 mm |
13.0 ft-lb/in @Thickness 0.500 in |
LW, Cond E-48/50; ASTM D256 |
Industrial Laminates/Norplex NP130HF Glass Fabric Description: High flexural, impact and tensile strength glass fabric epoxy laminate, especially in the machine direction. Engineered to provide better physical properties than NEMA FR-4. More dimens.. |
|||
Izod Impact, Unnotched | 6.94 J/cm @Thickness 12.7 mm |
13.0 ft-lb/in @Thickness 0.500 in |
LW, Cond E-48/50; ASTM D256 |
Industrial Laminates/Norplex NP511ES Glass Epoxy Laminate Description: NP511ES is a woven glass fabric with high temperature, static dissipative epoxy resin. It has excellent mechanical strength and electrical properties at elevated temperatures with a con.. |