Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 2.67 J/cm @Thickness 8.00 mm |
5.00 ft-lb/in @Thickness 0.315 in |
LW, E-48/50 |
Industrial Laminates/Norplex SP525M (WaveMax 5000) Glass Fabric Description: Non-woven substrate combined with high temperature, static dissipative epoxy resin. Superior machining properties. Capable of producing thin walls with high strength for finely machined.. |
|||
Izod Impact, Unnotched | 2.67 J/cm @Temperature -30.0 °C |
5.00 ft-lb/in @Temperature -22.0 °F |
ASTM D 4812 |
SABIC Innovative Plastics Noryl PX4058 PPE+PS PPO, polyolefin blend. Improved chemical resistance. 253F (125C) HDT.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Unnotched | 2.67 J/cm @Temperature -30.0 °C |
5.00 ft-lb/in @Temperature -22.0 °F |
ASTM D 4812 |
SABIC Innovative Plastics Noryl PX4058 PPE+PS (Asia Pacific) PPO, polyolefin blend. Improved chemical resistance. 253F (125C) HDT.This data was supplied by SABIC-IP for the Asia Pacific region. |