Polymer Property : Izod Impact, Unnotched = 4.81 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched 4.81 J/cm

@Thickness 12.7 mm
9.00 ft-lb/in

@Thickness 0.500 in
CW, Cond E-48/50; ASTM D256
Industrial Laminates/Norplex NP130HF Glass Fabric
Description: High flexural, impact and tensile strength glass fabric epoxy laminate, especially in the machine direction. Engineered to provide better physical properties than NEMA FR-4. More dimens..
Izod Impact, Unnotched 4.81 J/cm

@Thickness 12.7 mm
9.00 ft-lb/in

@Thickness 0.500 in
CW, Cond E-48/50; ASTM D256
Industrial Laminates/Norplex NP193M Synthetic Fabric Base Grade
Description: 17 oz. aramide and “soft glass” fibers are combined to make a fabric that is stronger than pure aramide and less abrasive than glass fabrics. This material is impregnated with..
Izod Impact, Unnotched 4.81 J/cm

@Thickness 12.7 mm
9.00 ft-lb/in

@Thickness 0.500 in
CW, Cond E-48/50; ASTM D256
Industrial Laminates/Norplex NP511 Glass Fabric
Description: Woven glass fabric with high temperature epoxy resin. Excellent mechanical strength and electrical properties at elevated temperatures. Continuous operating temperature is 165°C. Mat..
Izod Impact, Unnotched 4.81 J/cm

@Thickness 12.7 mm
9.00 ft-lb/in

@Thickness 0.500 in
CW, Cond E-48/50; ASTM D256
Industrial Laminates/Norplex NP511ES Glass Epoxy Laminate
Description: NP511ES is a woven glass fabric with high temperature, static dissipative epoxy resin. It has excellent mechanical strength and electrical properties at elevated temperatures with a con..