Mechanical Properties Metric English Comments
Izod Impact, Unnotched 4.54 J/cm

@Thickness 12.7 mm
8.50 ft-lb/in

@Thickness 0.500 in
LW, Cond E-48/50; ASTM D256
Industrial Laminates/Norplex NP192 Synthetic Fabric  (discontinued **)
Description: 8 oz. aramid and "soft glass" fibers are combined to make a fabric that is stronger than pure aramid and less abrasive than glass fabrics. This material is impregnated with a high tempe..
Izod Impact, Unnotched 4.54 J/cm

@Thickness 12.7 mm
8.50 ft-lb/in

@Thickness 0.500 in
CW, Cond E-48/50; ASTM D256
Industrial Laminates/Norplex NP509 Glass Fabric
Description: Woven glass fabric, melamine resin laminate. Very hard, flame resistant, machining grade with excellent electrical properties in high humidity conditions. High physical strength and exc..