Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 0.758 J/cm @Thickness 12.7 mm |
1.42 ft-lb/in @Thickness 0.500 in |
LW, Cond E-48/50; ASTM D256 |
Industrial Laminates/Norplex NP325 Cotton Fabric Description: Linen phenolic laminate with graphite added as a solid lubricant. Linen substrate provides better machining and wear resistance than NP315.Thickness Tested: 0.062", 0.125" and 0.500". |