Polymer Property : Izod Impact, Unnotched = 0.758 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched 0.758 J/cm

@Thickness 12.7 mm
1.42 ft-lb/in

@Thickness 0.500 in
LW, Cond E-48/50; ASTM D256
Industrial Laminates/Norplex NP325 Cotton Fabric
Description: Linen phenolic laminate with graphite added as a solid lubricant. Linen substrate provides better machining and wear resistance than NP315.Thickness Tested: 0.062", 0.125" and 0.500".