Mechanical Properties Metric English Comments
Izod Impact, Unnotched 0.686 J/cm

@Thickness 3.20 mm,
Temperature -30.0 °C
1.29 ft-lb/in

@Thickness 0.126 in,
Temperature -22.0 °F
ASTM D256
LG Chemical AF342T ABS, Flame Retardant, High Impact
Feature: Injection Molding, Flame Retardant, High ImpactApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 40039-93-8 and 1309-64-4Information provide..
Izod Impact, Unnotched 0.686 J/cm

@Thickness 6.40 mm,
Temperature -30.0 °C
1.29 ft-lb/in

@Thickness 0.252 in,
Temperature -22.0 °F
ASTM D256
LG Chemical AF360C ABS, TBBA-free Flame Retardant, High Flow
Feature: Injection Molding, TBBA-free Flame Retardant, High FlowApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9 and 1309-64-4Information provided by..
Izod Impact, Unnotched 0.686 J/cm

@Thickness 3.20 mm,
Temperature -30.0 °C
1.29 ft-lb/in

@Thickness 0.126 in,
Temperature -22.0 °F
ASTM D256
LG Chemical AF360C ABS, TBBA-free Flame Retardant, High Flow
Feature: Injection Molding, TBBA-free Flame Retardant, High FlowApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9 and 1309-64-4Information provided by..
Izod Impact, Unnotched 0.686 J/cm

@Thickness 6.40 mm,
Temperature -30.0 °C
1.29 ft-lb/in

@Thickness 0.252 in,
Temperature -22.0 °F
ASTM D256
LG Chemical AF360S ABS, TBBA-free Flame Retardant, Low Flow
Feature: Injection Molding, TBBA-free Flame Retardant, Low FlowApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 84852-53-9 and 1309-64-4Information ..
Izod Impact, Unnotched 0.686 J/cm

@Thickness 6.40 mm,
Temperature -30.0 °C
1.29 ft-lb/in

@Thickness 0.252 in,
Temperature -22.0 °F
ASTM D256
LG Chemical BM662B ABS, Heat Resistance
Feature: Blow Molding, Heat ResistanceApplication: Automotives Exterior Housing (Spoiler, Bumper Guard etc.)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 31621-07-5Information provided by LG Chemica..
Izod Impact, Unnotched 0.686 J/cm

@Thickness 3.20 mm,
Temperature -30.0 °C
1.29 ft-lb/in

@Thickness 0.126 in,
Temperature -22.0 °F
ASTM D256
LG Chemical BM662B ABS, Heat Resistance
Feature: Blow Molding, Heat ResistanceApplication: Automotives Exterior Housing (Spoiler, Bumper Guard etc.)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 31621-07-5Information provided by LG Chemica..
Izod Impact, Unnotched 0.686 J/cm

@Thickness 6.40 mm,
Temperature -30.0 °C
1.29 ft-lb/in

@Thickness 0.252 in,
Temperature -22.0 °F
ASTM D256
LG Chemical HI153 ABS, High Flow
Feature: Injection Molding, High Flow, Good WeatherabilityApplication: Electric & Electronic Products, Miscellaneous GoodsCAS No. 9003-56-9Information provided by LG Chemical
Izod Impact, Unnotched 0.686 J/cm

@Thickness 3.20 mm,
Temperature -30.0 °C
1.29 ft-lb/in

@Thickness 0.126 in,
Temperature -22.0 °F
ASTM D256
LG Chemical HI153 ABS, High Flow
Feature: Injection Molding, High Flow, Good WeatherabilityApplication: Electric & Electronic Products, Miscellaneous GoodsCAS No. 9003-56-9Information provided by LG Chemical
Izod Impact, Unnotched 0.686 J/cm

@Thickness 3.20 mm,
Temperature -30.0 °C
1.29 ft-lb/in

@Thickness 0.126 in,
Temperature -22.0 °F
ASTM D256
LG Chemical LG709W ABS, Low Gloss, Heat Resistance
Injection Molding, Low Gloss, Heat ResistanceApplication: Automobiles Interior Housing (Column Cover, Pilllars, Etc.)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 9003-54-7Information provided by LG..
Izod Impact, Unnotched 0.686 J/cm

@Thickness 3.20 mm,
Temperature -20.0 °C
1.29 ft-lb/in

@Thickness 0.126 in,
Temperature -4.00 °F
ASTM D256
LG Chemical MA210 ABS, Low Gloss
Feature: Extrusion Molding, General Purpose, Low GlossApplication: Automotive Sheet, Semi-Conductor TrayCAS No. 9003-56-9Information provided by LG Chemical
Izod Impact, Unnotched 0.686 J/cm

@Thickness 6.40 mm,
Temperature -30.0 °C
1.29 ft-lb/in

@Thickness 0.252 in,
Temperature -22.0 °F
ASTM D256
LG Chemical XR409H ABS, Heat Resistance
Feature: Injection Molding, Heat ResistanceApplication: Automotives Interior Housing (Switch Panel Housing etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7, and 31621-07-5Information provided by LG Ch..
Izod Impact, Unnotched 0.686 J/cm

@Thickness 3.20 mm,
Temperature -30.0 °C
1.29 ft-lb/in

@Thickness 0.126 in,
Temperature -22.0 °F
ASTM D256
LG Chemical XR409HJ ABS, Heat Resistance, Curl Fit
Feature: Injection Molding, Heat Resistance, Curl FitApplication: Automotives Interior & Exterior Housing (P/W Switch Housing Etc)CAS No. 25120-20-1, 9003-56-9 and 25747-74-7Information provided by ..
Izod Impact, Unnotched 0.686 J/cm

@Thickness 3.20 mm,
Temperature -30.0 °C
1.29 ft-lb/in

@Thickness 0.126 in,
Temperature -22.0 °F
ASTM D256
LG Chemical XR474 ABS, Heat Resistance
Feature: Injection Molding, Heat ResistanceApplication: Automotives Interior & Exterior HousingCAS No. 25120-20-1, 9003-56-9, 31621-07-5, and 9003-54-7Information provided by LG Chemical
Izod Impact, Unnotched 0.686 J/cm

@Thickness 6.40 mm,
Temperature -30.0 °C
1.29 ft-lb/in

@Thickness 0.252 in,
Temperature -22.0 °F
ASTM D256
LG Chemical AF308 ABS, Flame Retardant
Feature: Injection Molding, Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 40039-93-8 and 1309-64-4Information provided by LG Chemi..
Izod Impact, Unnotched 0.686 J/cm

@Thickness 3.20 mm,
Temperature -30.0 °C
1.29 ft-lb/in

@Thickness 0.126 in,
Temperature -22.0 °F
ASTM D256
LG Chemical AF308 ABS, Flame Retardant
Feature: Injection Molding, Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 40039-93-8 and 1309-64-4Information provided by LG Chemi..
Izod Impact, Unnotched 0.686 J/cm

@Thickness 3.20 mm,
Temperature -30.0 °C
1.29 ft-lb/in

@Thickness 0.126 in,
Temperature -22.0 °F
ASTM D256
LG Chemical AF360 ABS, TBBA-free Flame Retardant
Feature: Injection Molding, TBBA-free Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 84852-53-9 and 1309-64-4Information provided b..
Izod Impact, Unnotched 0.686 J/cm

@Thickness 6.40 mm,
Temperature -30.0 °C
1.29 ft-lb/in

@Thickness 0.252 in,
Temperature -22.0 °F
ASTM D256
LG Chemical XR401T ABS, Heat Resistance
Feature: Injection Molding, Heat ResistanceApplication: Electric & Electronic Housing (Frame etc) Automotives Interior & Exterior Housing (Garnish etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 9..
Izod Impact, Unnotched 0.686 J/cm

@Thickness 3.20 mm,
Temperature -30.0 °C
1.29 ft-lb/in

@Thickness 0.126 in,
Temperature -22.0 °F
ASTM D256
LG Chemical XR401T ABS, Heat Resistance
Feature: Injection Molding, Heat ResistanceApplication: Electric & Electronic Housing (Frame etc) Automotives Interior & Exterior Housing (Garnish etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 9..
Izod Impact, Unnotched 0.686 J/cm

@Thickness 3.20 mm,
Temperature -30.0 °C
1.29 ft-lb/in

@Thickness 0.126 in,
Temperature -22.0 °F
ASTM D256
LG Chemical XR404 ABS, Heat Resistance
Feature: Injection Molding, Heat ResistanceApplication: Electric & Electronic Housing (Frame etc) Automotives Interior & Exterior Housing (Garnish etc)CAS No. 25120-20-1, 9003-56-9 and 25747-74-7Inf..
Izod Impact, Unnotched 0.686 J/cm

@Thickness 6.40 mm,
Temperature -30.0 °C
1.29 ft-lb/in

@Thickness 0.252 in,
Temperature -22.0 °F
ASTM D256
LG Chemical XR404HJ ABS, Heat Resistance, Curl Fit
Feature: Injection Molding, Heat Resistance, Curl FitApplication: Automotives Interior Housing (P/W Switch Housing Etc)CAS No. 25120-20-1, 9003-56-9 and 25747-74-7Information provided by LG Chemica..
Izod Impact, Unnotched 0.686 J/cm

@Thickness 3.20 mm,
Temperature -30.0 °C
1.29 ft-lb/in

@Thickness 0.126 in,
Temperature -22.0 °F
ASTM D256
LG Chemical XR404T ABS, Heat Resistance
Feature: Injection Molding, Heat Resistance, Curl FitApplication: Automotives Interior Housing (P/W Switch Housing Etc)CAS No. 25120-20-1, 9003-56-9, and 9001-96-2Information provided by LG Chemical..
Copyright © lookpolymers.com All Rights Reserved