Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 0.347 J/cm @Thickness 12.7 mm |
0.650 ft-lb/in @Thickness 0.500 in |
LW, E-48/50 |
Industrial Laminates/Norplex NP631 Paper Base Laminate Description: Hot punching grade with excellent electrical properties and low moisture absorption.Thickness Tested: 0.062", 0.125" and 0.500" |
|||
Izod Impact, Unnotched | 0.347 J/cm @Thickness 12.7 mm |
0.650 ft-lb/in @Thickness 0.500 in |
LW, Cond E-48/50; ASTM D256 |
Industrial Laminates/Norplex NP639 Paper Base Laminate Description: Economical paper reinforced laminate developed with capacity to withstand temperatures to 150° C without blistering. High compressive strength and low moisture absorption.Thickness T.. |