Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 0.454 J/cm @Thickness 6.35 mm |
0.850 ft-lb/in @Thickness 0.250 in |
CW, E-48/50 |
Industrial Laminates/Norplex MC603 Paper Base Laminate
(discontinued **) Description: MC603 is constructed from electrical grade of kraft paper and a specially modified phenolic resin system, and is designed to be used in tap changers, coil support plates and terminal pa.. |