Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 0.400 J/cm @Thickness 12.7 mm |
0.750 ft-lb/in @Thickness 0.500 in |
LW, Cond E-48/50; ASTM D256 |
Industrial Laminates/Norplex NP660 Paper Base Laminate Description: Lower cost paper phenolic NEMA Grade XP. Uses natural kraft paper without pigmented cover sheet. Warm to hot punching. UL listed. Thickness Tested: 0.062", 0.125" & 0.500" |
|||
Izod Impact, Unnotched | 0.400 J/cm @Thickness 12.7 mm |
0.750 ft-lb/in @Thickness 0.500 in |
LW, Cond E-48/50; ASTM D256 |
Industrial Laminates/Norplex NP625 Paper Base Laminate Description: Paper phenolic grade with better moisture resistance than NP612. Requires less heat to punch and shear than NP611. |