Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 6.89 GPa @Temperature 23.0 °C |
999 ksi @Temperature 73.4 °F |
ASTM D790 |
Solvay Specialty Polymers Torlon® 4301 Polyamide-imide (PAI)
(Unverified Data**) Torlon 4301 is a wear-resistant grade of polyamide-imide (PAI) resin. It has a good balance of mechanical properties and wear resistance. It offers high flexural and compressive strength with a low .. |
|||
Flexural Modulus | 6.89 GPa @Temperature 23.0 °C |
999 ksi @Temperature 73.4 °F |
ASTM D790 |
Solvay Specialty Polymers Torlon® 4301 Polyamide-imide (PAI) Torlon® 4301 is a wear-resistant grade of polyamide-imide (PAI) resin. It has a good balance of mechanical properties and wear resistance. It offers high flexural and compressive strength with a .. |