Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 6.10 GPa @Temperature 23.0 °C |
885 ksi @Temperature 73.4 °F |
Absolute Drying; ASTM-D790 |
Toyobo GLAMIDE® T-422VOR Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |