Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 5.70 GPa @Temperature 23.0 °C |
827 ksi @Temperature 73.4 °F |
50%RH; ISO 178 |
DuPont Performance Polymers Zytel® 73G30T BK261 Nylon 6
(Unverified Data**) Zytel® 73G30T BK261 is a 30% glass fiber reinforced, toughened, black polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Flexural Modulus | 5.70 GPa @Temperature 23.0 °C |
827 ksi @Temperature 73.4 °F |
50%RH; ISO 178 |
DuPont Performance Polymers Zytel® 73G30T NC010 Nylon 6
(Unverified Data**) Zytel® 73G30T NC010 is a 30% glass fiber reinforced, toughened polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers |