Mechanical Properties Metric English Comments
Flexural Modulus 5.70 GPa

@Temperature 23.0 °C
827 ksi

@Temperature 73.4 °F
50%RH; ISO 178
DuPont Performance Polymers Zytel® 73G30T BK261 Nylon 6  (Unverified Data**)
Zytel® 73G30T BK261 is a 30% glass fiber reinforced, toughened, black polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers
Flexural Modulus 5.70 GPa

@Temperature 23.0 °C
827 ksi

@Temperature 73.4 °F
50%RH; ISO 178
DuPont Performance Polymers Zytel® 73G30T NC010 Nylon 6  (Unverified Data**)
Zytel® 73G30T NC010 is a 30% glass fiber reinforced, toughened polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers