Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 8.40 GPa @Temperature -40.0 °C |
1220 ksi @Temperature -40.0 °F |
Absolute Drying; ASTM-D790 |
Toyobo GLAMIDE® T-521 Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Flexural Modulus | 8.40 GPa @Temperature 23.0 °C |
1220 ksi @Temperature 73.4 °F |
DAM; ISO 178 |
DuPont Performance Polymers Zytel® FE5382 BK276 Nylon 612
(Unverified Data**) Zytel® FE5382 BK276 is a 33% glass fiber reinforced, heat stabilized, black polyamide 612 resin developed for electrical bobbins and encapsulation applications.Information provided by DuPont Perfor.. |