Mechanical Properties Metric English Comments
Flexural Modulus 3.93 GPa

@Temperature -40.0 °C
570 ksi

@Temperature -40.0 °F
50%RH; ASTM D790
DuPont Performance Polymers Zytel® 105F BK010 Nylon 66  (Unverified Data**)
Zytel® 105F BK010 is a lubricated, fast cycling, weather resistant PA 66 resin. Zytel® 105F BK010 contains finely dispersed carbon black.Information provided by DuPont Performance Polymers
Flexural Modulus 3.93 GPa

@Temperature 177 °C
570 ksi

@Temperature 350 °F
Master Bond EP45HT-1 Adhesive Resists Exposure to Sterilization
Description: Master Bond Polymer System EP45HT-1 is a remarkably fast curing, medium viscosity, two component epoxy compound formulated for high performance casting and bonding. It is 100% reactive ..