Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.350 GPa @Temperature 90.0 °C |
50.8 ksi @Temperature 194 °F |
ASTM D790 |
BASF Ultramid® 8202 L Intermediate PA6 (Dry) Description: Ultramid 8202 L-Intermediate is an unreinforced, low viscosity, non-lubricated PA6 injection molding homopolymer exhibiting excellent melt fluidity for filling thin sections. It is avai.. |