Mechanical Properties Metric English Comments
Flexural Modulus 5.00 GPa

@Temperature 150 °C
725 ksi

@Temperature 302 °F
Secant, 0.5 mm; ASTM D790
Premix Premi-Glas® 8101 Glass Reinforced Polyester BMC
Description: Premi-Glas® 8101 is a glass reinforced thermoset polyester Bulk Molding Compound designed for injection molding of automotive forward lighting reflectors. Key features and benefits: Ex..
Flexural Modulus 5.00 GPa

@Temperature 23.0 °C
725 ksi

@Temperature 73.4 °F
Practical Use (Water Absorption 2.5%); ASTM-D790
Toyobo GLAMIDE® T-402 Nylon-6
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Flexural Modulus 5.00 GPa

@Temperature 23.0 °C
725 ksi

@Temperature 73.4 °F
Practical Use (Water Absorption 2.3%); ASTM-D790
Toyobo GLAMIDE® T-422-02 Nylon-6
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Flexural Modulus 5.00 GPa

@Temperature 80.0 °C
725 ksi

@Temperature 176 °F
Practical Use (Water Absorption 1.0%); ASTM-D790
Toyobo GLAMIDE® TY-791GT 6T-Nylon
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..