Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 3.16 GPa @Temperature -40.0 °C |
458 ksi @Temperature -40.0 °F |
ASTM D790 |
BASF Ultramid® 8270 HS BK 102 PA6 (Dry) Description: Ultramid 8270 HS BK-102 is a thermally modified pigmented black, PA6 blow molding compound exhibiting exceptional toughness and melt strength ideally suited for blow molding, profile ex.. |