Mechanical Properties Metric English Comments
Flexural Modulus 23.0 GPa

@Temperature 150 °C
3340 ksi

@Temperature 302 °F
ISO 178
Vyncolit Neopreg Kinel® SK4525 S5 Glass Fiber Reinforced Molding Compound
BMI molding compound long glass fiber reinforced with excellent mechanical and thermal properties. Especially suited to be used for injection molding.Information provided by Sumitomo Bak North Ameri..