Mechanical Properties Metric English Comments
Flexural Modulus 3.80 GPa

@Temperature 23.0 °C
551 ksi

@Temperature 73.4 °F
Practical Use (Water Absorption 2.5%); ASTM-D790
Toyobo GLAMIDE® T-521 Nylon-6
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Flexural Modulus 3.80 GPa

@Temperature -40.0 °C
551 ksi

@Temperature -40.0 °F
Absolute Drying; ASTM-D790
Toyobo GLAMIDE® T-714E Transparent Nylon
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Flexural Modulus 3.80 GPa

@Temperature 23.0 °C
551 ksi

@Temperature 73.4 °F
Practical Use; ASTM-D790
Toyobo GLAMIDE® TY-835TC Nylon-66
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Flexural Modulus 3.80 GPa

@Temperature 23.0 °C
551 ksi

@Temperature 73.4 °F
Practical Use (Water Absorption 1.7%); ASTM-D790
Toyobo GLAMIDE® NB-5550 Nylon/Olefin
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Flexural Modulus 3.80 GPa

@Temperature 70.0 °C
551 ksi

@Temperature 158 °F
ASTM D790
DuPont Performance Polymers Delrin® 577 BK000 Acetal Homopolymer  (Unverified Data**)
Delrin® 577 BK000 is a medium viscosity acetal homopolymer containing 20% glass fiber filler, with high stiffness, low warpage and low creep for superior performance at elevated temperature. It con..