Polymer Property : Flexural Modulus = 3.10 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 3.10 GPa

@Temperature 23.9 °C
450 ksi

@Temperature 75.0 °F
ASTM D790
Saint-Gobain Meldin® 7001 CM Compression Molded Polyimide
Meldin® 7001 CM unfilled polyimide base resin, compression moldedSpecification Qualifications:Satisfies Type I P for ASTM D 6456-99: Standard Specification for Finished Parts Made from Polyimide ..
Flexural Modulus 3.10 GPa

@Temperature 80.0 °C
450 ksi

@Temperature 176 °F
Absolute Drying; ASTM-D790
Toyobo GLAMIDE® T-521 Nylon-6
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Flexural Modulus 3.10 GPa

@Temperature -40.0 °C
450 ksi

@Temperature -40.0 °F
Absolute Drying; ASTM-D790
Toyobo GLAMIDE® T-656E Nylon-66
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Flexural Modulus 3.10 GPa

@Temperature -40.0 °C
450 ksi

@Temperature -40.0 °F
Practical Use (Water Absorption 2.4%); ASTM-D790
Toyobo GLAMIDE® NB-1700 Nylon/Olefin
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Flexural Modulus 3.10 GPa

@Temperature 23.0 °C
450 ksi

@Temperature 73.4 °F
ISO 178
DuPont Performance Polymers Crastin® T835FRUV NC010 PBT
Crastin® T835FRUV NC010 is a 5% glass fiber reinforced, toughened, flame retardant polybutylene terephthalate resin for injection molding. (precommercial code = Crastin® CE2402)Information provide..
Flexural Modulus 3.10 GPa

@Temperature 23.0 °C
450 ksi

@Temperature 73.4 °F
ISO 178
DuPont Performance Polymers Delrin® 311DP NC010 Acetal Homopolymer  (Unverified Data**)
Delrin® 311DP is a medium-high viscosity acetal homopolymer with enhanced crystallization and balance of part performance and ease of processing. It has improved dimensional stability, high strengt..