Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.193 GPa @Temperature 23.0 °C |
28.0 ksi @Temperature 73.4 °F |
ASTM D790 |
DuPont Performance Polymers Hytrel® HTR6108 TPC-ET
(Unverified Data**) Hytrel® HTR6108 is a medium modulus grade, specially designed for good flexibility and low permeability to hydrocarbon fuels and oils. It has nominal hardness of 61D and can be processed by various.. |