Polymer Property : Flexural Modulus = 2500 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 17.2 GPa

@Temperature 71.1 °C
2500 ksi

@Temperature 160 °F
Wet; ASTM D790
Park Electrochemical Nelcote® E-761 Epoxy Prepreg, 120 E-Glass Reinforced
Nelcote® E-761 is a versatile self-adhesive epoxy matrix for use in aerospace and commercial application where ease of processing and cost are key considerations.Key Features and Benefits:Controlle..
Flexural Modulus 17.2 GPa

@Temperature 93.3 °C
2500 ksi

@Temperature 200 °F
Dry; ASTM D790
Park Electrochemical Nelcote® E-761 Epoxy Prepreg, 120 E-Glass Reinforced
Nelcote® E-761 is a versatile self-adhesive epoxy matrix for use in aerospace and commercial application where ease of processing and cost are key considerations.Key Features and Benefits:Controlle..
Flexural Modulus 17.2 GPa

@Temperature 23.9 °C
2500 ksi

@Temperature 75.0 °F
Dry; CMC form; ASTM D790
Park Electrochemical Nelcote® F-555 Phenolic Prepreg, C2 Reinforced
Nelcote® F-555 is a carbon-filled MIL-R-9299 phenolic resin optimized for coating Carbonized Rayon cloth. F-555 is used extensively in the manufacture of high temperature rocket nozzles, heat shiel..