Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 17.2 GPa @Temperature 71.1 °C |
2500 ksi @Temperature 160 °F |
Wet; ASTM D790 |
Park Electrochemical Nelcote® E-761 Epoxy Prepreg, 120 E-Glass Reinforced Nelcote® E-761 is a versatile self-adhesive epoxy matrix for use in aerospace and commercial application where ease of processing and cost are key considerations.Key Features and Benefits:Controlle.. |
|||
Flexural Modulus | 17.2 GPa @Temperature 93.3 °C |
2500 ksi @Temperature 200 °F |
Dry; ASTM D790 |
Park Electrochemical Nelcote® E-761 Epoxy Prepreg, 120 E-Glass Reinforced Nelcote® E-761 is a versatile self-adhesive epoxy matrix for use in aerospace and commercial application where ease of processing and cost are key considerations.Key Features and Benefits:Controlle.. |
|||
Flexural Modulus | 17.2 GPa @Temperature 23.9 °C |
2500 ksi @Temperature 75.0 °F |
Dry; CMC form; ASTM D790 |
Park Electrochemical Nelcote® F-555 Phenolic Prepreg, C2 Reinforced Nelcote® F-555 is a carbon-filled MIL-R-9299 phenolic resin optimized for coating Carbonized Rayon cloth. F-555 is used extensively in the manufacture of high temperature rocket nozzles, heat shiel.. |
|||
Flexural Modulus | 17.2 GPa @Temperature -40.0 °C |
2490 ksi @Temperature -40.0 °F |
Practical Use (Water Absorption 1.75%); ASTM-D790 |
Toyobo GLAMIDE® T-665C30 Nylon-66 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |