Mechanical Properties Metric English Comments
Flexural Modulus 14.5 GPa

@Temperature 23.0 °C
2100 ksi

@Temperature 73.4 °F
ASTM D790
Solvay Specialty Polymers Torlon® 4435 Polyamide-imide (PAI)  (Unverified Data**)
Torlon 4435 is a polyamide-imide resin specifically designed to provide exceptionally low wear performance in non-lubricated applications even at high pressure and velocity (PV) conditions. Not only..
Flexural Modulus 14.5 GPa

@Thickness 8.00 mm
2100 ksi

@Thickness 0.315 in
CW
Industrial Laminates/Norplex SP525M (WaveMax 5000) Glass Fabric
Description: Non-woven substrate combined with high temperature, static dissipative epoxy resin. Superior machining properties. Capable of producing thin walls with high strength for finely machined..
Flexural Modulus 14.5 GPa

@Temperature 23.0 °C
2100 ksi

@Temperature 73.4 °F
ASTM D790
Solvay Specialty Polymers Torlon® 4435 Polyamide-imide (PAI)
Torlon® 4435 is a polyamide-imide resin specifically designed to provide exceptionally low wear performance in non-lubricated applications even at high pressure and velocity (PV) conditions. Not ..
Flexural Modulus 14.5 GPa

@Temperature 23.0 °C
2100 ksi

@Temperature 73.4 °F
ASTM D790
Saint-Gobain Meldin® 5055 Thermoplastic Bearing Material
General Notes on Meldin 3000/5000 Series Bearing Products:Injection Moldable, High-Performance Bearings. Can withstand environments of high temperature, corrosive, and water.Specific Notes on Meldin..