Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 14.5 GPa @Temperature 23.0 °C |
2100 ksi @Temperature 73.4 °F |
ASTM D790 |
Solvay Specialty Polymers Torlon® 4435 Polyamide-imide (PAI)
(Unverified Data**) Torlon 4435 is a polyamide-imide resin specifically designed to provide exceptionally low wear performance in non-lubricated applications even at high pressure and velocity (PV) conditions. Not only.. |
|||
Flexural Modulus | 14.5 GPa @Thickness 8.00 mm |
2100 ksi @Thickness 0.315 in |
CW |
Industrial Laminates/Norplex SP525M (WaveMax 5000) Glass Fabric Description: Non-woven substrate combined with high temperature, static dissipative epoxy resin. Superior machining properties. Capable of producing thin walls with high strength for finely machined.. |
|||
Flexural Modulus | 14.5 GPa @Temperature 23.0 °C |
2100 ksi @Temperature 73.4 °F |
ASTM D790 |
Solvay Specialty Polymers Torlon® 4435 Polyamide-imide (PAI) Torlon® 4435 is a polyamide-imide resin specifically designed to provide exceptionally low wear performance in non-lubricated applications even at high pressure and velocity (PV) conditions. Not .. |
|||
Flexural Modulus | 14.5 GPa @Temperature 23.0 °C |
2100 ksi @Temperature 73.4 °F |
ASTM D790 |
Saint-Gobain Meldin® 5055 Thermoplastic Bearing Material General Notes on Meldin 3000/5000 Series Bearing Products:Injection Moldable, High-Performance Bearings. Can withstand environments of high temperature, corrosive, and water.Specific Notes on Meldin.. |