Mechanical Properties Metric English Comments
Flexural Modulus 20.7 GPa

@Temperature 21.1 °C
3000 ksi

@Temperature 70.0 °F
Wet; ASTM D790
Park Electrochemical Nelcote® E-761 Epoxy Prepreg, 7781 E-Glass Reinforced
Nelcote® E-761 is a versatile self-adhesive epoxy matrix for use in aerospace and commercial application where ease of processing and cost are key considerations.Key Features and Benefits:Controlle..
Flexural Modulus 20.7 GPa

@Temperature 71.0 °C
3000 ksi

@Temperature 160 °F
1/2 hr
Hexcel® HexPly® F515 Epoxy Resin, 1581 Glass Fabric
Hexcel designation: 1581-38"-F515; Fiber 150-1/2Information provided by HexCel
Copyright © lookpolymers.com All Rights Reserved