Polymer Property : Flexural Modulus = 16.2 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 0.112 GPa

@Temperature 23.0 °C
16.2 ksi

@Temperature 73.4 °F
ASTM D790
DuPont Performance Polymers Hytrel® HTR8136BK TPC-ET  (Unverified Data**)
Hytrel® HTR8136BK is designed for blow molding or processing by techniques requiring high melt viscosity. It has nominal durometer hardness of 49D, is pigmented black with fine particle size carbon..