Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 108.0 GPa @Temperature 22.8 °C |
15670 ksi @Temperature 73.0 °F |
Flexure Long; 15 min @ 250°F; prEN 2563 |
Hexcel® HexPly® EF01 Epoxy Curing System after THR 120 EF01 S25 38% Curing Cycle Information provided by HexCel |
|||
Flexural Modulus | 108.0 GPa @Temperature 22.8 °C |
15670 ksi @Temperature 73.0 °F |
Flexure Long; 30 min @ 250°F; prEN 2563 |
Hexcel® HexPly® EF01 Epoxy Curing System after THR 120 EF01 S25 38% Curing Cycle Information provided by HexCel |
|||
Flexural Modulus | 108.0 GPa @Temperature 50.0 °C |
15670 ksi @Temperature 122 °F |
Flexure Long; 30 min @ 250°F; prEN 2563 |
Hexcel® HexPly® EF01 Epoxy Curing System after THR 120 EF01 S25 38% Curing Cycle Information provided by HexCel |