Mechanical Properties Metric English Comments
Flexural Modulus 108.0 GPa

@Temperature 22.8 °C
15670 ksi

@Temperature 73.0 °F
Flexure Long; 15 min @ 250°F; prEN 2563
Hexcel® HexPly® EF01 Epoxy Curing System after THR 120 EF01 S25 38% Curing Cycle
Information provided by HexCel
Flexural Modulus 108.0 GPa

@Temperature 22.8 °C
15670 ksi

@Temperature 73.0 °F
Flexure Long; 30 min @ 250°F; prEN 2563
Hexcel® HexPly® EF01 Epoxy Curing System after THR 120 EF01 S25 38% Curing Cycle
Information provided by HexCel
Flexural Modulus 108.0 GPa

@Temperature 50.0 °C
15670 ksi

@Temperature 122 °F
Flexure Long; 30 min @ 250°F; prEN 2563
Hexcel® HexPly® EF01 Epoxy Curing System after THR 120 EF01 S25 38% Curing Cycle
Information provided by HexCel