Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Flexural Modulus = 155 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 1.07 GPa

@Temperature 23.0 °C
155 ksi

@Temperature 73.4 °F
50%RH; ISO 178
DuPont Performance Polymers Zytel® FG42A NC010 Nylon 66  (Unverified Data**)
Zytel® FG42A NC010 is a high viscosity polyamide 66 resin for injection molding and extrusion. It has been developed for consideration into applications such as parts for the food industry.Informat..
Copyright © lookpolymers.com All Rights Reserved