Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.07 GPa @Temperature 23.0 °C |
155 ksi @Temperature 73.4 °F |
50%RH; ISO 178 |
DuPont Performance Polymers Zytel® FG42A NC010 Nylon 66
(Unverified Data**) Zytel® FG42A NC010 is a high viscosity polyamide 66 resin for injection molding and extrusion. It has been developed for consideration into applications such as parts for the food industry.Informat.. |