Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 15.2 GPa

@Temperature 71.1 °C
2200 ksi

@Temperature 160 °F
Wet; ASTM D790
Park Electrochemical Nelcote® E-761 Epoxy Prepreg, 4581 Quartz
Nelcote® E-761 is a versatile self-adhesive epoxy matrix for use in aerospace and commercial application where ease of processing and cost are key considerations.Key Features and Benefits:Controlle..
Flexural Modulus 15.2 GPa

@Temperature 93.3 °C
2200 ksi

@Temperature 200 °F
Dry; ASTM D790
Park Electrochemical Nelcote® V-341 Polybutadiene Prepreg, 503 Quartz Reinforced
Nelcote® V-341 is Polybutadiene resin system designed to provide excellent electrical properties in demanding airborne, shipboard, and undersea applications.Key Features and Benefits:Extremely low ..
Flexural Modulus 15.2 GPa

@Thickness 8.00 mm
2200 ksi

@Thickness 0.315 in
LW
Industrial Laminates/Norplex SP525M (WaveMax 5000) Glass Fabric
Description: Non-woven substrate combined with high temperature, static dissipative epoxy resin. Superior machining properties. Capable of producing thin walls with high strength for finely machined..
Flexural Modulus 15.2 GPa

@Temperature 23.0 °C
2200 ksi

@Temperature 73.4 °F
50%RH; ISO 178
DuPont Performance Polymers Zytel® HTN FR52G45BL BK337 Polyphthalamide (PPA)  (Unverified Data**)
Zytel® HTNFR52G45BL BK337 is a 45% glass reinforced, flame retardant, lubricated high performance polyamide resin that has been developed for connector applications.Information provided by DuPont ..
Flexural Modulus 15.2 GPa

@Temperature 23.0 °C
2200 ksi

@Temperature 73.4 °F
DAM; ISO 178
DuPont Performance Polymers Zytel® HTN FR52G45BL BK337 Polyphthalamide (PPA)  (Unverified Data**)
Zytel® HTNFR52G45BL BK337 is a 45% glass reinforced, flame retardant, lubricated high performance polyamide resin that has been developed for connector applications.Information provided by DuPont ..