Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 7.58 GPa @Thickness 1.57 mm |
1100 ksi @Thickness 0.0620 in |
LW |
Industrial Laminates/Norplex NP631 Paper Base Laminate Description: Hot punching grade with excellent electrical properties and low moisture absorption.Thickness Tested: 0.062", 0.125" and 0.500" |
|||
Flexural Modulus | 7.60 GPa @Temperature 23.0 °C |
1100 ksi @Temperature 73.4 °F |
DAM; ISO 178 |
DuPont Performance Polymers Zytel® 80G33HS1L BK104 Nylon 66
(Unverified Data**) Zytel® 80G33HS1L BK104 is a 33% glass fiber reinforced, heat stabilized black polyamide 66 resin with outstanding impact resistance developed using DuPont Super Tough technology.Information provide.. |