Polymer Property : Flexural Modulus = 0.290 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 0.00200 GPa

@Temperature 100 °C
0.290 ksi

@Temperature 212 °F
dry
Zotefoams ZOTEK® N B50 High Performance Nylon Foam
Zotek® N B50 is a closed cell, cross-linked polyamide-6 foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs..
Flexural Modulus 0.00200 GPa

@Temperature 0.000 °C
0.290 ksi

@Temperature 32.0 °F
conditioned
Zotefoams ZOTEK® N B50 High Performance Nylon Foam
Zotek® N B50 is a closed cell, cross-linked polyamide-6 foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs..
Flexural Modulus 0.00200 GPa

@Temperature 50.0 °C
0.290 ksi

@Temperature 122 °F
conditioned
Zotefoams ZOTEK® N B50 High Performance Nylon Foam
Zotek® N B50 is a closed cell, cross-linked polyamide-6 foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs..