Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.0600 GPa @Temperature 100 °C |
8.70 ksi @Temperature 212 °F |
ASTM D790 |
DuPont Performance Polymers Hytrel® HTR6108 TPC-ET
(Unverified Data**) Hytrel® HTR6108 is a medium modulus grade, specially designed for good flexibility and low permeability to hydrocarbon fuels and oils. It has nominal hardness of 61D and can be processed by various.. |
|||
Flexural Modulus | 0.0600 GPa @Temperature 100 °C |
8.70 ksi @Temperature 212 °F |
ISO 178 |
DuPont Performance Polymers Hytrel® HTR6108 TPC-ET
(Unverified Data**) Hytrel® HTR6108 is a medium modulus grade, specially designed for good flexibility and low permeability to hydrocarbon fuels and oils. It has nominal hardness of 61D and can be processed by various.. |