Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.0120 GPa @Temperature -40.0 °C |
1.74 ksi @Temperature -40.0 °F |
dry |
Zotefoams ZOTEK® N B50 High Performance Nylon Foam Zotek® N B50 is a closed cell, cross-linked polyamide-6 foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs.. |