Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.000200 GPa @Temperature 200 °C |
0.0290 ksi @Temperature 392 °F |
dry |
Zotefoams ZOTEK® N B50 High Performance Nylon Foam Zotek® N B50 is a closed cell, cross-linked polyamide-6 foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs.. |
|||
Flexural Modulus | 0.000200 GPa @Temperature 200 °C |
0.0290 ksi @Temperature 392 °F |
conditioned |
Zotefoams ZOTEK® N B50 High Performance Nylon Foam Zotek® N B50 is a closed cell, cross-linked polyamide-6 foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs.. |