Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Gardner Impact = 8.83543 J Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Gardner Impact 8.83543 - 8.83543 J

@Temperature -28.9 - -28.9 °C
6.51667 - 6.51667 ft-lb

@Temperature -20.0 - -20.0 °F
Average value: 8.84 J Grade Count:1
Overview of materials for Ethylene Butyl Acrylate
This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Butyl Acrylate". Each property range of values reported is minimum and maximum values of approp..
Gardner Impact 8.83543 - 8.83543 J

@Thickness 3.17 - 3.17 mm
6.51667 - 6.51667 ft-lb

@Thickness 0.125 - 0.125 in
Average value: 8.84 J Grade Count:1
Overview of materials for Ethylene Butyl Acrylate
This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Butyl Acrylate". Each property range of values reported is minimum and maximum values of approp..