Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Gardner Impact | 8.83543 - 8.83543 J @Temperature -28.9 - -28.9 °C |
6.51667 - 6.51667 ft-lb @Temperature -20.0 - -20.0 °F |
Average value: 8.84 J Grade Count:1 |
Overview of materials for Ethylene Butyl Acrylate This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Butyl Acrylate". Each property range of values reported is minimum and maximum values of approp.. |
|||
Gardner Impact | 8.83543 - 8.83543 J @Thickness 3.17 - 3.17 mm |
6.51667 - 6.51667 ft-lb @Thickness 0.125 - 0.125 in |
Average value: 8.84 J Grade Count:1 |
Overview of materials for Ethylene Butyl Acrylate This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Butyl Acrylate". Each property range of values reported is minimum and maximum values of approp.. |