Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Gardner Impact = 30.2 ft-lb Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Gardner Impact 40.9 J

@Temperature 22.0 °C
30.2 ft-lb

@Temperature 71.6 °F
ASTM D5420
KYDEX® 2200LT Thermoplastic Sheet for Mass Transit Applications
Features:Meets flamespread and smoke development requirements listed in 49 CFR 238Excellent formability and fabrication characteristicsAllows for tight tolerance controlsExcellent resistance to graf..