Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Gardner Impact | 16.5 J @Temperature -30.0 °C |
12.2 ft-lb @Temperature -22.0 °F |
ASTM D5420 |
Washington Penn Medium Impact Copolymer Grades are available to meet FDA food and drug packaging requirements. These products have excellent mold detail and surface reproduction with fast set-up times. They are also available in an array .. |