Washington Penn Medium Impact Copolymer

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Washington Penn
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Washington Penn Medium Impact Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Grades are available to meet FDA food and drug packaging requirements. These products have excellent mold detail and surface reproduction with fast set-up times. They are also available in an array of colors.Information provided by Washington Penn Plastic Co.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D792
Filler Content 0.00 %
0.00 %
Mechanical Properties Metric English Comments
Tensile Strength, Yield 22.4 MPa
3250 psi
ASTM D638
Elongation at Break 545 %
545 %
ASTM D638
Elongation at Yield 16 %
16 %
ASTM D638
Flexural Modulus 1.00 GPa
145 ksi
1% Secant; ASTM D790
1.03 GPa
150 ksi
Tangent; ASTM D790
Izod Impact, Notched 1.23 J/cm
2.30 ft-lb/in
ASTM D256
Gardner Impact 16.5 J

@Temperature -30.0 °C
12.2 ft-lb

@Temperature -22.0 °F
ASTM D5420
24.4 J

@Temperature 23.0 °C
18.0 ft-lb

@Temperature 73.4 °F
ASTM D5420
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 73.9 °C
165 °F
ASTM D648