Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop, Total Energy | 35.0 J @Temperature -30.0 °C |
25.8 ft-lb @Temperature -22.0 °F |
ASTM D3763 |
SABIC Innovative Plastics Cycoloy® CM6240 PC+ABS (Asia Pacific) CYCOLOY CM6240 resin is a flame retardant PC/ABS blend featuring balanced properties of high modulus, good flow and ductility. It is of Br- & Cl-free flame retardant systems intended to meet thin wa.. |
|||
Dart Drop, Total Energy | 35.0 J @Temperature 23.0 °C |
25.8 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics GELOY CR7520 ASA General purpose ASA. Excellent weatherability, good flow/aesthetics and high impact. Rated F2 by UL. |
|||
Dart Drop, Total Energy | 35.0 J @Temperature 23.0 °C |
25.8 ft-lb @Temperature 73.4 °F |
ISO 6603-2 |
Borealis Borpact™ SG910MO Polypropylene for Injection Molding Borpact™ SG910MO is a high impact and transparent polypropylene. This grade provides high gloss, high transparency and excellent impact properties. Applications: containers and products with medium.. |