Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Borealis Borpact™ SG910MO Polypropylene for Injection Molding

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Borealis
Trade Name Borpact™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Borealis Borpact™ SG910MO Polypropylene for Injection Molding.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Borpact™ SG910MO is a high impact and transparent polypropylene. This grade provides high gloss, high transparency and excellent impact properties. Applications: containers and products with medium to long flow length, houseware goods with high impact and transparency at ambient and low temperatures, transparent storage crates and boxes (House wares), transparent crates and boxes for industrial handling systems, transparent packaging where high impact is needed (i.e. pails), and technical articles where transparency and impact is needed (i.e. covers).Information provided by Borealis AG
Physical Properties Metric English Comments
Density 0.905 g/cc
0.0327 lb/in³
ISO 1183
Linear Mold Shrinkage 0.010 - 0.020 cm/cm
0.010 - 0.020 in/in
Melt Flow 25 g/10 min

@Load 2.16 kg,
Temperature 230 °C
25 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Rockwell R 67
67
ISO 2039-2
Tensile Strength, Yield 23.0 MPa
3340 psi
ISO 527-2
Elongation at Yield 14 %
14 %
ISO 527-2
Tensile Modulus 0.900 GPa
131 ksi
ISO 527-2
Charpy Impact, Notched 0.200 J/cm²

@Temperature -10.0 °C
0.952 ft-lb/in²

@Temperature 14.0 °F
ISO 179/1eA
0.400 J/cm²

@Temperature 0.000 °C
1.90 ft-lb/in²

@Temperature 32.0 °F
ISO 179/1eA
0.800 J/cm²

@Temperature 23.0 °C
3.81 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Dart Drop, Total Energy 5.00 J

@Temperature -10.0 °C
3.69 ft-lb

@Temperature 14.0 °F
ISO 6603-2
20.0 J

@Temperature 0.000 °C
14.8 ft-lb

@Temperature 32.0 °F
ISO 6603-2
35.0 J

@Temperature 23.0 °C
25.8 ft-lb

@Temperature 73.4 °F
ISO 6603-2
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 72.0 °C
162 °F
ISO 75-2
Optical Properties Metric English Comments
Haze 21 %
21 %
1mm plaque; Borealis Method
Transmission, Visible 90 %
90 %
transparent; thickness not quantified
Processing Properties Metric English Comments
Melt Temperature 220 - 260 °C
428 - 500 °F
Mold Temperature 20.0 - 40.0 °C
68.0 - 104 °F
Hold Pressure 20.0 - 50.0 MPa
2900 - 7250 psi
Descriptive Properties Value Comments
Injection Velocity high
Copyright © lookpolymers.com All Rights Reserved