Mechanical Properties Metric English Comments
Rupture Strength 97.0 MPa

@Temperature 815 °C,
Time 360000 sec
14100 psi

@Temperature 1500 °F,
Time 100 hour
Initial Stress
Haynes X-750 Nickel Alloy Sheet and Strip (AMS 5598, UNS N07750)
Haynes X-750 (UNS No. N07750) alloy is an age-hardenable, nickel-base superalloy with very good strength at temperatures up to about 1600°F (870°C). It is widely used as a wrought material for..
Rupture Strength 97.0 MPa

@Temperature 871 °C,
Time 3.60e+6 sec
14100 psi

@Temperature 1600 °F,
Time 1000 hour
Plate
Haynes 282® Nickel Alloy Sheet, Plate and Bar, Solution Annealed
Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la..
Copyright © lookpolymers.com All Rights Reserved