Polymer Property : Rupture Strength = 93.0 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Rupture Strength 93.0 MPa

@Temperature 700 °C,
Time 3.60e+7 sec
13500 psi

@Temperature 1290 °F,
Time 10000 hour
Stress Rupture
AFE Technologies Cronite Standard Nickel Alloy Castings, No. HR4
High temperature nickel alloy castings. Applications include heat treatment and handling products, furnace products, tubes, power generation, and petrochemical industries.Information provided by AF..