Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Rupture Strength | 93.0 MPa @Temperature 700 °C, Time 3.60e+7 sec |
13500 psi @Temperature 1290 °F, Time 10000 hour |
Stress Rupture |
AFE Technologies Cronite Standard Nickel Alloy Castings, No. HR4 High temperature nickel alloy castings. Applications include heat treatment and handling products, furnace products, tubes, power generation, and petrochemical industries.Information provided by AF.. |