Polymer Property : Rupture Strength = 84800 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Rupture Strength 585 MPa

@Temperature 600 °C,
Time 360000 sec
84800 psi

@Temperature 1110 °F,
Time 100 hour
Initial Stress
Haynes X-750 Nickel Alloy Sheet and Strip (AMS 5598, UNS N07750)
Haynes X-750 (UNS No. N07750) alloy is an age-hardenable, nickel-base superalloy with very good strength at temperatures up to about 1600°F (870°C). It is widely used as a wrought material for..
Rupture Strength 585 MPa

@Temperature 649 °C,
Time 3.60e+6 sec
84800 psi

@Temperature 1200 °F,
Time 1000 hour
Special Metals UDIMET® alloy 520 Superalloy
UDIMET® alloy 520 is a precipitation-hardenable nickel base superalloy with an exceptional combination of high-temperature mechanical properties, corrosion resistance and forgeability characteris..